Customization: | Available |
---|---|
Thickness: | 23mm |
Style: | European |
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
New Production Technique
Compared to the traditional product, 3D embossing product will have more natural visual effect and more realistic wood grain texture. 3D embossing technique do not need a follow-up treatment, it can finish the embossing procedure during the extrusion technique.
Long-termed Durability
The grain texture of 3D embossing can provide long-termed durability because it is deeper than the normal embossing. The abrasion during the application is not so obvious as the normal embossing.
PROPERTY |
Test Method |
VALUE |
UNIT |
1. Density |
ASTM D792-2008 METHOD B |
1.285 |
g / cm 3 |
2. Flexural Modul u s |
ASTM D790-07E1 |
3070 |
Mpa |
3. Flexural Strength |
ASTM D790-07E1 |
38 |
Mpa |
4. Water Absorption |
ASTM D570-98 |
0.18 |
% |
5. Linear Thermal Expansion Coefficient |
ASTM E831-06 |
49.82 |
UM/M °C |
6. IZOD Impact Strength |
ASTM D4812-06 |
79 |
J/m |
7. Hardness |
ASTM D2240-05 |
D/76/1 |
|
8.UV Resistance (Light Resistance / Xenon-Arc Exposure) |
IS0105-02:2000/Amd.2:2000(E), ISO 05-A02:1993 Cor2:2005, Exposure 720 hours |
Grey 4-5 grey scale Brown 4 grey scale Mahogany 4-5 grey scale Dark Walnut 4-5 grey scale |
/ |
9.Thermal Shock Test |
IEC 60068-2-14 Na: 1986, 5 cycles |
No signs of cracking, warping, chipping and discoloration |
/ |
10.Mould Resistance |
ASTM F609 |
First Grade |
/ |
1. We will control Quality and delivery time strictly.
2. Timely follow up about the feedbacks from customers.
3. Provide professional advice for your engineering design.
4. Supply technical guidance for installation.